Solar pile corrosion & 30-year ASTM A123 coating life checker

Screen galvanized pile life against your soil report: corrosivity class, zinc exhaustion year, bare-steel loss and the remaining web at end of design life.

Soil & pile inputs

ohm-cm (Wenner 4-pin or soil box)
below 5.5 or above 10 accelerates zinc loss
ppm
ppm
Soil corrosivity class
–
Zinc depletion rate
–
Zinc exhaustion
–
Bare steel loss
–
Remaining web
–
Engineering screening verdict
–

Spec upgrades, side by side

OptionSpecificationZinc lifeWeb at end of lifeVerdict
Attach to a bid request

Screening only. Sacrificial thickness and coating are set by the project P.E. from site soil tests.

How the checker calculates

Galvanized piles corrode in two stages. First the zinc is consumed, at a rate set mainly by soil resistivity. Then bare carbon steel corrodes from both faces of the web. The checker estimates when the zinc runs out, how many years of bare-steel loss fall inside the design life, and how much web is left at the end.

Soil resistivityClassZinc lossµm/yr
> 10,000 ohm-cmMild / non-corrosive0.08–0.16 mils/yr2–4
5,000–10,000 ohm-cmMild–moderate0.16–0.31 mils/yr4–8
2,000–5,000 ohm-cmModerate0.31–0.47 mils/yr8–12
< 2,000 ohm-cmAggressive / corrosive0.47–0.85+ mils/yr12–22+
Empirical underground zinc loss on hot-dip galvanized steel.

Multipliers

  • pH: +35% per pH unit below 5.5, +40% per unit above 10.
  • Chlorides: up to +80% at 2,000 ppm.
  • Sulfates: up to +50% at 3,000 ppm.
  • Moisture: ×0.85 well-drained, ×1.0 seasonal, ×1.3 saturated.

Coatings and bare steel

ASTM A123 requires a minimum average of 3.9–4.7 mils on structural shapes; 4.3 mils is used as the typical average. Reactive silicon/phosphorus steel can reach 5.5–7.5+ mils (6.0 used). Pre-galvanized G235 sheet carries about 2.0 mils per side. Zn-Al-Mg coatings are modelled at 40% of the zinc loss rate. The soil-air collar option cuts zinc and steel loss at the grade line, where corrosion usually governs. Bare carbon steel loses about 0.35–1.9 mils per year per side across the resistivity range, scaled by the same multipliers.

Verdict thresholds

Pass: at least 85% of the original web remains at end of design life. Marginal: 70–85%. High risk: below 70%. Structural adequacy depends on the section modulus actually required by the racking loads, so treat these as screening flags for the engineer of record, not a design check.

Section properties for every profile are on driven W-beam piles. For C-piles versus W-beams in corrosive ground, see roll-formed C-piles.

Send the pile schedule. Get a foundation bid.

MWdc, racking, geotech status and mobilization window are enough to start. Steel supply, driving crews, ground screws, pre-drilling and load testing priced as one package or line by line.